P.V.D. COATING SPECIFICATIONS
TPVD TiCN


TPVD TiCN Coating

Tanury's titanium carbonitride (TiCN) coatings produced with the proprietary cathodic arc physical vapor deposition (PVD) process.

TPVD TiCN coatings provide higher hardness and lower coefficient of friction than titanium nitride (TiN). TPVD TiCNi coating is designed for wear applications. Its coefficient of friction is superior to that of TPVD TiN while its hardness and adhesion are comparable.




TPVD TiCN PROPERTIES
Hardness (HV 0.05)
Upper Critical Load (N)
Oxidation Temp. (¼C)
Friction Coefficient
Surface Roughness (Raµm)
Color
4200 ± 200
70
400
0.32
0.15
Blue-Black

FEATURES
High Hardness
Coefficient of Friction
Extends Wear Resistance
Coating Thickness = 0.25µm to 5µm
Excellent Adhesion Low
Good Toughness